MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultraform® W 2320 003 BK120 Q600 POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Ultraform W 2320 003 BK120 Q600 is a pigmented black, very easy flowing and rapidly solidifying injection molding POM grade for use where processing is extremely difficult but mechanical properties are lower. Contains a mold release agent. It conforms to FDA requirements of 21 CFR 177.2470.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccISO 1183
Water Absorption 0.80 %ISO 62
Moisture Absorption at Equilibrium 0.20 %23°C/50% R.H.; ISO 62
Linear Mold Shrinkage 0.019 cm/cmASTM Data; MD
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 63.0 MPa50mm/min; ISO 527
Elongation at Yield 7.5 %50mm/min; ISO 527
Tensile Modulus 2700 MPa1mm/min; ISO 527
Flexural Modulus 2600 MPaISO Data
Izod Impact, Notched (ISO) 5.50 kJ/m²ISO Test
Charpy Impact, Notched 0.550 J/cm²ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 167 °C10 K/min
 167 °CASTM Test
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °CISO 75
 
Compliance PropertiesOriginal ValueComments
FDA Yes21 CFR 177.2470
 
Descriptive Properties
ColorBK120
Commercial StatusActive America
Impact ModifiedNo
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultraform® W 2320 003 UNC Q600 POM
BASF Ultraform® N 2320 003 UNC Q600 POM
BASF Ultraform® H 2320 006 Q600 POM
BASF Ultraform® N2320 0035 LEV POM
BASF Ultraform® W2320 U03 POM

PBASF9112 / 84876

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.