VESTAKEEP® Care is the ideal materials for the fabrication of medical devices with short time contact to human blood, tissue or bone for up to 30 days. VESTAKEEP® Care Grades have a good biocompatibility, processability and the option to pigment. VESTAKEEP® Care M20 G black is a medium viscosity, unreinforced polyether ether ketone for injection molding. The semi-crystalline polymer features superior thermal and chemical resistance. Dry properties listed below Industrial Sector: Medical Devices Processing: Injection molding Delivery form: Pellets, Granules Resistance to: Heat (thermal stability), Hydrolysis / hot water, Wear / abrasion, Fatigue resistance Conformity: Biocompatibility, Medical application Additives: Unfilled Applications: Encapsulation Special Characteristics: Semi-crystalline Regulatory: US Pharmacopeia Class VI conformity Color: Black Chemical Resistance: Acid resistance, Alkali resistance, Solvent resistance, Grease resistance, Hydrolytically stable, Oil resistance, Oxidation resistance, General chemical resistanceInformation provided by Evonik. |