MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Henkel Loctite® Stycast® US 1195 Two-Component Urethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Loctite Stycast US 1195 provides the following product characteristics:
  • High Hardness
  • Mineral-filled
  • Low Tg

Cure: Room temperature cure followed by heat cure

Application: Potting and Encapsulating

Typical Assembly Applications: Circuit Board Protection, Automotive electronic applications or Telecommunication devices

Loctite Stycast US 1195 is formulated for potting electronics or devices for protection against environmental hazards. This material exhibits high hardness compared to other urethane materials allowing improved durability and impact resistance. It's low Tg allows for better thermal cycle performance to meet low temperature requirements in harsh environments.

Loctite Stycast US 1195 passed internal flammability testing at 3 mm thickness.

Information provided by Henkel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³Part A
 1.43 g/cc0.0517 lb/in³Mixed
 1.45 g/cc0.0524 lb/in³Part B
Brookfield Viscosity 55 cP55 cPPart A; RVF
 19000 cP19000 cPMixed; Spindle 51, speed 5.0 rpm
 40000 cP40000 cPSpindle 51, speed 5.0 rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9191
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 9.60e+14 ohm-cm9.60e+14 ohm-cm
Dielectric Constant  3.63
@Frequency 1e+6 Hz
3.63
@Frequency 1e+6 Hz
 3.7
@Frequency 100000 Hz
3.7
@Frequency 100000 Hz
Dielectric Strength 42.0 kV/mm
@Thickness 20.0 mm
1070 kV/in
@Thickness 0.787 in
Dissipation Factor  0.0342
@Frequency 100000 Hz
0.0342
@Frequency 100000 Hz
 0.1208
@Frequency 1e+6 Hz
0.1208
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear  58.0 µm/m-°C
@Temperature <=-75.0 °C
32.2 µin/in-°F
@Temperature <=-103 °F
Below Tg
 128 µm/m-°C
@Temperature >=-75.0 °C
71.1 µin/in-°F
@Temperature >=-103 °F
Above Tg
Thermal Conductivity 0.670 W/m-K4.65 BTU-in/hr-ft²-°FLaser Flash
Glass Transition Temp, Tg -75.0 °C-103 °FTMA
 
Processing PropertiesMetricEnglishComments
Cure Time 240 min
@Temperature 65.0 °C
4.00 hour
@Temperature 149 °F
Gel Time 30.0 min30.0 min
Shelf Life 6.00 Month6.00 MonthPart A, from date of manufacture
 6.00 Month6.00 MonthPart B, from date of manufacture
 
Descriptive Properties
AppearanceBlackMixed
 Black PastePart B
 Dark Brown LiquidPart A
Mix Ratio, by Volume13.45 : 100Part A : Part B
Mix Ratio, by Weight11.5 : 100Part A : Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHENK7966 / 255450

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.