TABOREN-PM 29 T 20-027 is a compound based on mixture of polypropylene block copolymer and polypropylene homopolymer filled with 20% of talc, stabilized with a high antioxidant package. It is suitable for extrusion and blow molding applications in many industrial fields with stress put on excellent processability and good surface performance.Information provided by Silon US LLC. |