MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
RSP Technology RSA-443 AE Aluminum Super Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy

Material Notes: Precision Equipment, Optics

Features: CTE match with Nickel and stainless steel, low density, specific stiffness, high thermal conductivity

Applications:

  • Mirror body with Ni-coating
  • Electronic packaging, heat sinks, Carriers, guidance and fixtures bars for PCB
  • Gimbal systems, optical mounts, wave guides
  • Microscope stages, spectrometer parts, air bearings, measurement devices
  • Semiconductor substrates, wafers

Replacing: Titanium, Stainless steel, CuW, Kovar, Invar, Conventional al alloys like 6061, 6082, 5083

RSP Technology develops, produces and sells aluminium super alloys with high end properties. By using its own Meltspinning process, ultra fast cooling rates can be reached, converting more than 1 million degrees per second. As a result very fine nanostructured alloys with new functionalities are being developed and produced.

Information provided by RSP Technology BV

Vendors: RSP Technology – Aluminum as strong as Titanium For more information contact: +31 (0)596 632 300 or visit www.rsp-technology.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.54 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 105
Tensile Strength, Ultimate 240 MPa
Tensile Strength, Yield 150 MPa
Elongation at Break 1.5 %
Tensile Modulus 102.1 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.5 µm/m-°C
Thermal Conductivity 135 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 60 %
Silicon, Si 40 %
 
Descriptive Properties
Specific Stiffness40GPa/(g/cc)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik Osprey CE11 Al-Si Controlled Expansion Alloy
RSP Technology RSA-6061 T6 Aluminum Super Alloy
Sandvik Osprey CE13 Al-Si Controlled Expansion Alloy
RSP Technology RSA-441 T6 Aluminum Super Alloy
Aluminum 7075-T6; 7075-T651

NRSP21 / 100835

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.