MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
AMT AM-Lite® Die Casting Magnesium Alloy  (discontinued **)
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: AM-lite is a high surface finish die casting alloy suitable for applications that currently utilize zinc, aluminum or magnesium (alloy AZ91D) die castings, or plastic injection moldings. AM-lite has better die casting properties than existing magnesium alloys, plus an improved as-cast surface finish that is suitable for decorative surface finishing operations. A special electroplating process has been developed for AM-Lite to take advantage of these properties.

MatWeb has no current information about the producer, Advanced Magnesium Technologies (AMT).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.02 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 76 - 80
Hardness, Vickers 85 - 90300 g
Tensile Strength, Ultimate 230 - 250 MPa
Tensile Strength, Yield 160 - 170 MPa
@Strain 0.2 %
Elongation at Break 3.0 - 4.0 %
Creep Strength 35.0 MPa
@Temperature 150 °C,
Time 720000 sec
0.2% strain
 60.0 MPa
@Temperature 150 °C,
Time 720000 sec
0.5% strain
Modulus of Elasticity 45.3 GPa
Compressive Yield Strength 150 MPa0.2% proof
Compressive Strength 446 MPa
Poissons Ratio 0.35
Fatigue Strength 85.0 MPa
@# of Cycles 5.00e+7
R.R.Moore
 181 MPa
@# of Cycles 1.00e+6
3 point bend; R=0.1
Shear Modulus 16.8 GPa
Charpy Impact 3.30 J10x10 mm, Unnotched
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000105 - 0.000110 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 340 J/g
CTE, linear 24.9 µm/m-°C
Specific Heat Capacity 0.950 J/g-°C
Thermal Conductivity 83.0 W/m-K
Melting Point 330 - 585 °C
Solidus 330 °C
Liquidus 585 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Magnesium AZ91D-F, Cast
Aluminum 384.0-F Die Casting Alloy
Aluminum A360.0-F Die Casting Alloy
Aluminum 1100-H18
405 Stainless Steel

NMAGN00 / 89270

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.