MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay GEROPON® AF 71 Surfactant
Categories: Fluid

Material Notes: Description: "GEROPON AF 71 is powdered Foam Control Agent that has been developed for construction industry. GEROPON AF 71 depresses the formation of undesired air bubbles in building products, based on hydraulic binders, during their make-up process and working. The highflowability of GEROPON AF 71 permits an easy incorporation in dry blends, or aqueous pastes with very low air content. It is universally applicable and in use both in neutral and alkaline systems, besides it shows good compatibility with other additives such as water soluble surfactants or polymers."

Identification: SURFACE ACTIVE AGENT FIXED ON INERT CARRIER

Available in: Asia Pacific, Europe, Latin America and North America

Solubility: Dispersible in water. Insoluble in polar adn aromatic solvents.

Applications: GEROPON AF 71 is powdered Foam Control Agent that has been developed for construction industry. GEROPON AF 71 depresses the formation of undesired air bubbles in building products, based on hydraulic binders, during their make-up process and working. The high flowability of GEROPON AF 71 permits an easy incorporation in dry blends, or aqueous pastes with very low air content. It is universally applicable and in use both in neutral and alkaline systems, besides it shows good compatibility with other additives such as water soluble surfactants or polymers.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.430 g/cc
pH 7.0 - 8.55% in water; RPG02
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 100 °C
 
Descriptive Properties
AppearanceWhite, free flowing powderRPG31
CompositionActive content0.5
Ionic ChargeNonionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay GEROPON® CYA/75 Surfactant
Verdant Specialty Solutions MACKADET® 40-K Surfactant
Solvay GEROPON® DA Surfactant
Solvay MACKADET® DR-100M Surfactant
Solvay MACKADET® CA-ND Surfactant

WRHOD118 / 137349

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.