MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chambroad Petrochemicals TF-MWP
Categories: Other Engineering Material

Material Notes: Highly Absorbent Fabric: The highly absorbent fabrics have three series. Among them, the oil-absorbing fabric, made of lipophilic microfiber nonwovens, absorb soil but not water, and can absorb a large amount of oil quickly; the general-purpose absorbent fabric has undergone special hydrophilicity treatment, can quickly absorb a large amount of oil, water, coolant, pigment, and dye; the chemical absorbing fabric has undergone special inert treatment, can withstand corrosion, acid, and alkali, and quickly absorb a large amount of chemical solvent.

Application Field: Oil Absorbing Fabric - After absorbing oil, the product can float in the water, thereby being suitable for the treatment of grease in the water.

Information provided by Shandong Chambroad Petrochemicals Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Composite force>35Ntransversal, at rupture
 >43Nlongitudinal, at rupture
Liquid absorption<1 mintime
Oil<1 minabsorbency time
 >10absorption rate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHAMB036 / 318578

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.