MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Superior Flux Superior Sybergel Flux and Cleaner
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • A VOC-Free flux and cleaner.
  • Non-halide formulation.
  • A water washable cleaner that eliminates the need for organic solvents.
  • Compatible with all cored solders.
  • Completely free of rosins, resins and petroleum derivatives.
  • Non-hazardous and safe to handle.
  • Waterless, odorless, non-spattering liquid.
  • Formulated for use with tin/lead and lead-free alloys.
Description: SyberGel Flux and Cleaner is a dual purpose product for manual soldering applications. It is 1) a gel flux that promotes excellent solderability and 2) a cleaner that removes rosin and all organic and inorganic residues from electronic assemblies. It smokes less than current products and is a non-hazardous, VOC-Free compound that contains no rosin and is water-soluble. SyberGel Flux and Cleaner is compatible with all core solders. In particular, when using rosin core solders, operators can clean post solder residues with water and need no solvents to remove residues. Another radical departure from traditional hand-soldering techniques the usage of SyberGel for solder removal, touch-up, device removal and re-attachment. SyberGel Flux and Cleaner simplifies board repair and touch-up procedures, while promoting excellent solder coverage, shiny joints, and cleaning without using environmentally hazardous solvents.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/cc
Density 1.16 g/cc0.0419 lb/in³
pH 1.8 - 3.21.8 - 3.2
Viscosity 140000 cP140000 cP
 
Thermal PropertiesMetricEnglishComments
Flash Point 177 °C351 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 95.0 - 315 °C203 - 599 °FSoldering Range
Shelf Life 2.00 Month2.00 Month
 
Descriptive Properties
FormTranslucent Gel
Rosin Solubility33.9%
Spread Factor>80

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NSFLUX128 / 185812

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.