Hiprolon® 90 MC HLS G30 is a polyamide 6.12 compound reinforced with 30% chopped glass fiber, and is used for injection molding. Features: high dimension stability, chemical resistance, impact resistance; widely used for auto parts, quick connectors, housing et al;Information provided by Suzhou Hipro Polymers Co. Ltd., subsequently acquired by Arkema S.A. |