MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Seals Eastern 7182E Fluorocarbon-Elastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Formulated AFLAS® high-temperature "sour" oil & gas service. Excellent acid and base resistance.

Information provided by Seals Eastern, Inc.

Key Words: FEPM
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.56 g/cc1.56 g/ccASTM D297, 15
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A >= 84>= 84ASTM D2240, Type A
 8989AVG; ASTM D2240, Type A
 88
@Treatment Temp. 200 °C,
Time 1.21e+6 sec
88
@Treatment Temp. 392 °F,
Time 336 hour
After Dry Heat Aging; ASTM D865
 89
@Treatment Temp. 200 °C,
Time 3.60e+6 sec
89
@Treatment Temp. 392 °F,
Time 1000 hour
After Dry Heat Aging; ASTM D865
Tensile Strength at Break >= 16.8 MPa>= 2430 psiASTM D412 Method A
 21.59 MPa3131 psiAVG; ASTM D412 Method A
 20.51 MPa
@Treatment Temp. 200 °C,
Time 3.60e+6 sec
2974 psi
@Treatment Temp. 392 °F,
Time 1000 hour
After Dry Heat Aging; ASTM D865
 23.75 MPa
@Treatment Temp. 200 °C,
Time 1.21e+6 sec
3444 psi
@Treatment Temp. 392 °F,
Time 336 hour
After Dry Heat Aging; ASTM D865
Tensile Stress at Strain  4.60 MPa
@Strain 25 %
667 psi
@Strain 25 %
Average; ASTM D412 Method A
 >= 4.77 MPa
@Strain 50 %
>= 692 psi
@Strain 50 %
Minimum; ASTM D412 Method A
 7.715 MPa
@Strain 50 %
1119 psi
@Strain 50 %
Average; ASTM D412 Method A
 >= 9.31 MPa
@Strain 100 %
>= 1350 psi
@Strain 100 %
Minimum; ASTM D412 Method A
 13.95 MPa
@Strain 100 %
2023 psi
@Strain 100 %
Average; ASTM D412 Method A
Elongation at Break >= 120 %>= 120 %ASTM D412 Method A
 174 %174 %AVG; ASTM D412 Method A
 244 %
@Treatment Temp. 200 °C,
Time 3.60e+6 sec
244 %
@Treatment Temp. 392 °F,
Time 1000 hour
After Dry Heat Aging; ASTM D865
 273 %
@Treatment Temp. 200 °C,
Time 1.21e+6 sec
273 %
@Treatment Temp. 392 °F,
Time 336 hour
After Dry Heat Aging; ASTM D865
Tear Strength Test 359359(psi); ASTM D624, Die B
Compression Set 21 %
@Temperature 200 °C,
Time 79200 sec
21 %
@Temperature 392 °F,
Time 22.0 hour
ASTM D395, Test B
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 2.78 °C37.0 °FASTM D1329
 
Processing PropertiesMetricEnglishComments
Shelf Life 240 Month240 MonthASTM D395, Test B
 
Descriptive Properties
Strain Energy / Unit Volume at 20% Elongation (psi)68

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Seals Eastern 7182X Fluorocarbon-Elastomer
Seals Eastern 7182D Fluorocarbon-Elastomer
Seals Eastern 7182B Fluorocarbon-Elastomer
Seals Eastern 7182A Fluorocarbon-Elastomer
Carpenter Pyrotough® 78 Hot Work Die Steel

PSEAL38 / 80185

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.