SBR 1769 is an environmentally friendly version of SBR 1721 with the highest bound styrene content, and a naphthenic oil extender oil. It was developed for tire applications. Unique Features: - Cold polymerized styrene-butadiene elastomer
- Highest bound styrene and naphthenic oil extender
Applications:- Passenger & heavy-service treads
- Retread rubbers and bicycle tires
Information provided by Lion Elastomer |