MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECANYL VH2 Black Polyphenylene oxide
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO

Material Notes:
  • excellent dimensional stability
  • very good chemical resistance
  • flame retardant according to UL94 V-0
  • low smoke emissions
  • low moisture absorption
  • good electrically insulating
Target Industries:
  • aircraft and aerospace interiors
  • aircraft and aerospace technology
  • Railway Interiors
  • transportation

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.12 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 7690 psiASTM D 638
Tensile Strength, Yield 9280 psiASTM D 638
Modulus of Elasticity 322 ksiASTM D 638
Flexural Strength 14500 psiASTM D 790
Flexural Modulus 342000 psiASTM D 790
Izod Impact, Unnotched 5.60 ft-lb/inASTM D 256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 252 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.50 mm
Flame Spread Index 15ASTM E 162
Glow Wire Ignition Temperature 775 °C
@Thickness 1.00 mm
ASTM 60695-2
 775 °C
@Thickness 1.50 mm
ASTM 60695-2
 775 °C
@Thickness 2.00 mm
ASTM 60695-2
 800 °C
@Thickness 3.00 mm
ASTM 60695-2
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
ASTM 60695-2
 
Descriptive Properties
Colorblack
Flammability11-13 PassesASTM E 662 (Air/Rail) Ds @ 1.5 min; FAR 25.853
 20-40 passesASTM E 662 (Air/Rail) Ds @ 4.0 min; FAR 25.853
 73-106 Meets FAR RequirementsASTM E 662 (Air/Rail) Ds @ 20 min
 Passes3 mm; 60 sec. Vertical Bunsen Burner test FAR 25.853; Appx F, Prt 1, (a), 1, (Air)
 PassesFAA Smoke Density Test (resin data); FAR 25.853 Appx F, Prt 1, (a), 1, (Air)
 PassesToxicity - Draeger Tube (resin data); FAR 25.853 Appx F, Prt 1, (a), 1, (Air)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENSIN8176 / 319104

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.