MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

NMG ProCell® PC100 PVC Foam Core
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoplastic; Vinyl (PVC); PVC, Foam Grade

Material Notes: ProCell® is used in as a core in a variety of composites areas. It can be used in closed molding processes, such hand lay-up and vacuum infusion, etc. ProCell is made mainly from PVC with closed cells and a cross-linked structure. It has extremely high specific strength, specific stiffness and good toughness.

Information provided by NMG Composites Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.100 g/cc0.00361 lb/in³ISO 845
Water Absorption 1.0 %1.0 %ISO 2896
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 2.69 MPa390 psiASTM–C297
Elongation at Break 34 %34 %Shear elongation; ISO 1922
Tensile Modulus 0.125 GPa18.1 ksiASTM–C297
Compressive Strength 1.86 MPa270 psiASTM- D 1621
Compressive Modulus 0.134 GPa19.4 ksiASTM- D 1621
Shear Modulus 0.0350 GPa5.08 ksiASTM-C273
Shear Strength 1.64 MPa238 psiASTM-C273
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0350 W/m-K0.243 BTU-in/hr-ft²-°FISO 8301
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNMG903 / 230584

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.