Titanpro SM398 is a clarified grade designed for high transparency articles. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adjuvant meet their respective FDA regulations and 21 CFR 177.1520(b). In summary, this resin meets the FDA criteria covering safe use of polyolefin articles and component of articles intended for food contact use. TSCA Registry: CAS# 9010-79-1 Applications: - High transparency containers
- Housewares
- Stationeries
Advantages:- Excellent clarity
- Low blooming
- Good surface finish and color
- Cycle time reduction with low processing melt temperature
- Utilities cost saving
- Good balance of rigidity and impact resistance
Fabrication: Equipment - ram and screw injection machines Techniques - standard processingInformation provided by Titan Chemical |