MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akrochem AKROCHEM® Peptizer 66
Categories: Other Engineering Material

Material Notes: Product Description: Peptizer 66 is an activated 2,2’-dibenzamido diphenyldisulfide (DBDD) absorbed on a clay carrier. It can be used as processing aids/viscosity reducers for natural and synthetic rubbers.

Applications: Peptizer 66 is an effective chemical peptizers primarily used for natural rubber. Recommended dosage levels in natural rubber range from 0.05 to 0.5 phr (as final mixing temperature increases, the lower levels should be used). Synthetic rubbers require approximately 2.0 phr. More specific dosage recommendations are included on page 2 of this data sheet. Benefits of using Peptizer 66:

  • lower viscosity/improved processing
  • lower dump temperatures with subsequent mixing
  • improved mold flow
  • improved uniformity of extrusions and calendared sheets
  • little effect on vulcanizate properties vs. mechanically masticated rubber
  • acceptable under FDA regulation 21 CFR 177.2600

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.83 g/cc
Ash 47 %
 
Descriptive Properties
Appearanceoff white powder
Content0.4Active DBDD

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH550 / 315468

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.