MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sandvik 18.8.Mn Welding wire
Categories: Metal; Ferrous Metal; Austenitic

Material Notes: Sandvik 18.8.Mn is a filler material of ER 307 type suitable for joining work hardenable steels, armour plates, austenitic stainless manganese steels and free machining steels (such as ASTM 303) and stainless Cr steels with max. 18% Cr. The grade is used in, for example, the automotive industry for joining dissimilar steels. It is also suitable for overlay welding on carbon and low alloy steels. Sandvik 18.8.Mn is available as wire and rods for MIG/MAG, TIG and plasma arc welding.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 200200
Tensile Strength, Ultimate 650 MPa94300 psi
Tensile Strength, Yield 460 MPa
@Strain 0.2 %
66700 psi
@Strain 0.2 %
Elongation at Break 41 %41 %
Reduction of Area 61 %61 %
Charpy Impact 140 J103 ft-lb
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  15.0 W/m-K
@Temperature 20.0 °C
104 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 16.0 W/m-K
@Temperature 100 °C
111 BTU-in/hr-ft²-°F
@Temperature 212 °F
 18.0 W/m-K
@Temperature 300 °C
125 BTU-in/hr-ft²-°F
@Temperature 572 °F
 20.0 W/m-K
@Temperature 500 °C
139 BTU-in/hr-ft²-°F
@Temperature 932 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.070 %0.070 %All-Weld metal
 0.080 %0.080 %AIM
Chromium, Cr 18 %18 %AIM
 18 %18 %All-Weld metal
Cobalt, Co <= 0.50 %<= 0.50 %AIM
Copper, Cu <= 0.10 %<= 0.10 %AIM
Manganese, Mn 6.0 %6.0 %All-Weld metal
 7.0 %7.0 %AIM
Molybdenum, Mo <= 0.30 %<= 0.30 %AIM
Nickel, Ni 8.0 %8.0 %AIM
 8.0 %8.0 %All-Weld metal
Nitrogen, N 0.050 %0.050 %All-Weld metal
 <= 0.060 %<= 0.060 %AIM
Phosphorus, P 0.010 %0.010 %All-Weld metal
 <= 0.025 %<= 0.025 %AIM
Silicon, Si 0.80 %0.80 %All-Weld metal
 0.90 %0.90 %AIM
Sulfur, S 0.010 %0.010 %All-Weld metal
 <= 0.015 %<= 0.015 %AIM

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ASTM A662 Carbon Steel, Grade A
China Tungsten YWR2 Tungsten Carbide with Rare Earth Additive
China Tungsten YT730 Tungsten Carbide
Victrex VICOTE™ F805 Polyetheretherketone (PEEK) Liquid Dispersion
Victrex VICOTE™ F804 Black Polyetheretherketone (PEEK) Liquid Dispersion

NSANDV5078 / 199642

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.