MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Zinc Slush Casting Alloy A (Zn-4.75Al-0.25Cu)
Categories: Metal; Nonferrous Metal; Zinc Alloy

Material Notes: Properties are for chill cast samples.

Key Words: ASTM B792; UNS Z34510
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 6.50 g/cc0.235 lb/in³Estimated by MatWeb
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 193 MPa28000 psi
Elongation at Break 1.0 %1.0 %in 5 cm
Charpy Impact, Unnotched 4.00 J2.95 ft-lb
 
Thermal PropertiesMetricEnglishComments
Melting Point 380 - 390 °C716 - 734 °F
Solidus 380 °C716 °F
Liquidus 390 °C734 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 4.5 - 5.0 %4.5 - 5.0 %
Cadmium, Cd <= 0.0050 %<= 0.0050 %
Copper, Cu 0.20 - 0.30 %0.20 - 0.30 %
Iron, Fe <= 0.10 %<= 0.10 %
Lead, Pb <= 0.0070 %<= 0.0070 %
Tin, Sn <= 0.0050 %<= 0.0050 %
Zinc, Zn 94.583 - 95.3 %94.583 - 95.3 %As balance; Ingot per ASTM B 792

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ArcelorMittal 14 High formability steel for drawing, Hot rolled
ASTM A588 HSLA Steel Grade B, Thickness < 100 mm (4 in.)
Commercial Rolled Zinc (Zn-0.3Pb-0.03Cd; UNS Z21540), Hot-Rolled
Morgan Advanced Ceramics Mac-35 Au/65 Cu-WM Braze Alloy
Oxygen-free electronic Copper, UNS C10100

MZNSLA / 14568

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.