MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRICOMP™ Compound DL003EXJ Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP LUBRICOMP DL003EXJ compound is based on Polycarbonate (PC) resin containing 15% PTFE. Added features of this grade include: Easy Molding, Low Extractable, Wear Resistant, Healthcare.

Features: Low Extractable,Healthcare,Wear resistant,Food Contact Acceptable,Easy Molding

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.29 g/ccASTM D792
Density 1.29 g/ccASTM D792
Moisture Absorption 0.0200 %Injection Molding
 0.100 %23°C/50% RH/24 hrs; ASTM D570
 0.150 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 34.0 MPa5 mm/min; ISO 527
 38.0 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 45.0 MPa5 mm/min; ISO 527
 46.0 MPa5 mm/min; ASTM D638
Elongation at Break 17.3 %5 mm/min; ASTM D638
 21.8 %5 mm/min; ISO 527
Elongation at Yield 5.4 %5 mm/min; ISO 527
 5.6 %5 mm/min; ASTM D638
Tensile Modulus 1980 MPa1 mm/min; ISO 527
 2090 MPa50 mm/min; ASTM D638
Flexural Strength 67.0 MPaISO 178
Flexural Modulus 2000 MPa2 mm/min; ISO 178
 2190 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 176 JASTM D256
Izod Impact, Unnotched 1780 J/mASTM D4812
Izod Impact, Notched (ISO) 12.0 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 110 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 33.0 JASTM D3763
Impact Test 28.0 JMultiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.38ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.23ASTM D3702 Modified: Manual
K (wear) Factor 15.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 77.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
CTE, linear, Transverse to Flow 77.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 141 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 141 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 124 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 130 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Zone 2 305 - 315 °C
Zone 3 310 - 320 °C
Melt Temperature 300 - 315 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 120 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80742 / 288689

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.