MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Akrochem AKROWAXES™ 195 Microcrystalline Wax
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Akrowax 195 is a fully refined microcrystalline wax derived from petroleum in bead form. This particular wax will migrate very slowly to the surface of a rubber part. For this reason it should not be used alone for ozone protection but combined with a low melt paraffin wax to provide a flexible antiozonant film. Typically, Akrowax 195 is used in the sealants industry where the wax’s ease of incorporation, firmness below melt point (roughly defined melt point is approximately 195?F) and flow properties are all advantageous. The high molecular weight gives this wax high melt point and firmness at room temperature. This wax complies with F.D.A. Regulations for use as indirect or direct food additives described in Code of Federal Regulations, Title 21, Chapter 1, Section 172.886 and 178.3710 as well as 177.2600, Rubber Articles Intended For Repeated Use.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Melting Point 76.7 - 85.0 °C170 - 185 °FCongealing Point; ASTM D938
Dropping Point 88.9 - 100 °C192 - 212 °F
 
Descriptive Properties
AppearanceBead

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH632 / 315550

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.