MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Evonik COUPSIL® VP 6508 Precipitated silica
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Precipitated silica, surface-modified with organosilane DYNASYLAN® VTEO for application in the rubber industry.

Description: Reaction product of organosilane DYNASYLAN® VTEO [Vinyltriethoxysilan] and ULTRASIL® VN 2 (specific surface area 130 m2/g). The product consists of 100 parts of ULTRASIL® VN 2 modified with 8 parts of DYNASYLAN® VTEO. Since the reaction between the organosilane and the silica is nearly completed, COUPSIL® VP 6508 offers the advantage of a homogeneous modification with low moisture adsorption during storage and significantly lower development of ethanol during mixing and processing.

Applications and properties: COUPSIL® VP 6508 is used as a reinforcing filler in rubber compounds. It reacts with unsaturated polymers during vulcanization under formation of covalent chemical bonds. This imparts greater tensile strength, higher moduli, reduced compression set, increased abrasion resistance and optimized dynamic properties. COUPSIL® VP 6508 is used in peroxide cured rubber compounds in combination with white fillers and where optimum technical properties are required.

Application fields are: Mechanical rubber goods

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.220 g/cc0.00795 lb/in³Tamped
Volatiles 4.0 %4.0 %
pH >= 7.2>= 7.2ISO 789-9
 
Descriptive Properties
Appearancewhite powder
Silane content0.078

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIN005 / 317039

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.