MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Teknor Apex Vital-Line SMM3707 Rigid Polyvinyl Chloride
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: Availability: Asia Pacific. Form : pellets. Features: ethylene oxide sterilizable, non-phthalate plasticizer. Processing Method: injection molding. Uses: medical / healthcare applications.

Typical temperature profile for processing compound is from 145°C to 180°C. The optimum temperatures depend on the type of machine as well as screw design being used to process. Feeding zone: 145°C, compression zone: 140-155°C, mold temperature: 0°C-50°C, nozzle zone: 170-185°C, Barrel zone: 150-170°C..

Information provided by Teknor Apex.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7878ASTMD2240
Tensile Strength, Yield 35.0 MPa5080 psi20 in/min; ASTM D638
Elongation at Break 100 %100 %ASTM D638
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 80.0 °C176 °FASTM D1525
 
Descriptive Properties
Heat Stability> 30 min, ASTM D2115-92, 374°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Colorite Polymers 2019F Rigid PVC
Geon® Performance Solutions Vinyl Packaging XPL319 Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Rigid Extrusion L0259
Geon® Performance Solutions Vinyl Rigid Extrusion LR840 Polyvinyl Chloride, Rigid
Teknor Apex APEX® RE 8114 UV Polyvinyl Chloride, Rigid

PTEKNN9656 / 231057

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.