MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Titanium 11 (Ti-6Al-2Sn-1.5Zr-1Mo-0.35Bi-0.1Si), Aged
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Near Alpha Titanium Alloy

Material Notes: Sample Annealed 705ºC then aged 595ºC.

Applications: High-temp jet engines. Blades, discs, spacers, seals. High performance automotive valves.

1 other heat treatment of this alloy is in MatWeb.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 4.50 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1040 MPa
Tensile Strength, Yield 940 MPa
Elongation at Break 19 %
Reduction of Area 32 %
Modulus of Elasticity 115 GPaTypical value for an alpha titanium alloy
Poissons Ratio 0.31Typical for alpha titanium alloy.
Shear Modulus 43.9 GPaCalculated from typical values.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000160 ohm-cmEstimated from similar alpha titanium alloys.
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.00 µm/m-°C
@Temperature 20.0 - 100 °C
Typical alpha titanium alloy
Specific Heat Capacity 0.525 J/g-°CTypical value for titanium alloys.
Thermal Conductivity 7.00 W/m-KEstimated from similar titanium alloys.
Beta Transus 1000 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 6.0 %
Bismuth, Bi 0.35 %
Molybdenum, Mo 1.0 %
Silicon, Si 0.10 %
Tin, Sn 2.0 %
Titanium, Ti 89 %
Zirconium, Zr 1.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Fibre Glast 549 Kevlar® Fabric
Titanium Ti-6Al-2Sn-4Zr-2Mo-0.1Si; Duplex Annealed
Titanium 11 (Ti-6Al-2Sn-1.5Zr-1Mo-0.35Bi-0.1Si)
Titanium Ti-11.5Mo-6Zr-4.5Sn, ST 720°C, Aged 495°C
ATI Allvac® 6-2-4-2 Titanium Alloy, Heat Treatment: 982°C (1800°F) + Age

MTA111 / 14116

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.