MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Solvay Chemicals 5% - Technical Grade Hydrochloric acid
Categories: Fluid

Material Notes: Supplied with HCl content of 33% to 36% by weight; property data specifically for HCl aqueous solution diluted to 5%. Hydrochloric acid, also known as muriatic acid, is a colorless to yellow liquid, with a pungent odor. Hydrochloric acid is a strong acid used as chemical reagent, pH-regulating, ion exchanger regenerating, pickling or cleaning agent.

EINECS: 231-595-7/CAS: 7647-01-0/UN: 1789

Information provided by Solvay

Key Words: Muriatic Acid
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity  0.30 cP
@Temperature 100 °C
0.30 cP
@Temperature 212 °F
Dynamic Viscosity
 0.38 cP
@Temperature 80.0 °C
0.38 cP
@Temperature 176 °F
Dynamic Viscosity
 0.51 cP
@Temperature 60.0 °C
0.51 cP
@Temperature 140 °F
Dynamic Viscosity
 0.72 cP
@Temperature 40.0 °C
0.72 cP
@Temperature 104 °F
Dynamic Viscosity
 1.1 cP
@Temperature 20.0 °C
1.1 cP
@Temperature 68.0 °F
Dynamic Viscosity
 1.4 cP
@Temperature 10.0 °C
1.4 cP
@Temperature 50.0 °F
Dynamic Viscosity
 1.84 cP
@Temperature 0.000 °C
1.84 cP
@Temperature 32.0 °F
Dynamic Viscosity
Molecular Weight 36.47 g/mol36.47 g/molHCl
Vapor Pressure  0.00600 bar
@Temperature 0.000 °C
4.50 torr
@Temperature 32.0 °F
 0.0120 bar
@Temperature 10.0 °C
9.00 torr
@Temperature 50.0 °F
 0.0220 bar
@Temperature 20.0 °C
16.5 torr
@Temperature 68.0 °F
 0.0700 bar
@Temperature 40.0 °C
52.5 torr
@Temperature 104 °F
 0.190 bar
@Temperature 60.0 °C
143 torr
@Temperature 140 °F
 0.450 bar
@Temperature 80.0 °C
338 torr
@Temperature 176 °F
 0.970 bar
@Temperature 100 °C
728 torr
@Temperature 212 °F
Surface Tension  0.061 dynes/cm
@Temperature 100 °C
0.061 dynes/cm
@Temperature 212 °F
 0.064 dynes/cm
@Temperature 80.0 °C
0.064 dynes/cm
@Temperature 176 °F
 0.067 dynes/cm
@Temperature 60.0 °C
0.067 dynes/cm
@Temperature 140 °F
 0.070 dynes/cm
@Temperature 40.0 °C
0.070 dynes/cm
@Temperature 104 °F
 0.073 dynes/cm
@Temperature 20.0 °C
0.073 dynes/cm
@Temperature 68.0 °F
 0.074 dynes/cm
@Temperature 10.0 °C
0.074 dynes/cm
@Temperature 50.0 °F
 0.075 dynes/cm
@Temperature 0.000 °C
0.075 dynes/cm
@Temperature 32.0 °F
 0.076 dynes/cm
@Temperature -10.0 °C
0.076 dynes/cm
@Temperature 14.0 °F
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity  3.80 J/g-°C
@Temperature 0.000 °C
0.908 BTU/lb-°F
@Temperature 32.0 °F
 3.80 J/g-°C
@Temperature 10.0 °C
0.908 BTU/lb-°F
@Temperature 50.0 °F
 3.80 J/g-°C
@Temperature 20.0 °C
0.908 BTU/lb-°F
@Temperature 68.0 °F
 3.90 J/g-°C
@Temperature 40.0 °C
0.932 BTU/lb-°F
@Temperature 104 °F
 3.90 J/g-°C
@Temperature 60.0 °C
0.932 BTU/lb-°F
@Temperature 140 °F
 3.90 J/g-°C
@Temperature 80.0 °C
0.932 BTU/lb-°F
@Temperature 176 °F
 3.90 J/g-°C
@Temperature 100 °C
0.932 BTU/lb-°F
@Temperature 212 °F
Thermal Conductivity  0.550 W/m-K
@Temperature 0.000 °C
3.82 BTU-in/hr-ft²-°F
@Temperature 32.0 °F
 0.560 W/m-K
@Temperature 10.0 °C
3.89 BTU-in/hr-ft²-°F
@Temperature 50.0 °F
 0.570 W/m-K
@Temperature 20.0 °C
3.96 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 0.600 W/m-K
@Temperature 40.0 °C
4.16 BTU-in/hr-ft²-°F
@Temperature 104 °F
 0.620 W/m-K
@Temperature 60.0 °C
4.30 BTU-in/hr-ft²-°F
@Temperature 140 °F
 0.640 W/m-K
@Temperature 80.0 °C
4.44 BTU-in/hr-ft²-°F
@Temperature 176 °F
 0.670 W/m-K
@Temperature 100 °C
4.65 BTU-in/hr-ft²-°F
@Temperature 212 °F
Melting Point -6.00 °C21.2 °F
Boiling Point 101 °C
@Pressure 0.101 MPa
214 °F
@Pressure 14.6 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WSOLV138s / 234798

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.