MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman Eastotac™ C-115L Resin
Categories: Polymer

Material Notes: Product Description: Eastotac™ C-115L Resin is a tackifier resin with a ring and ball softening point of 115°C and a molten Gardner color of 2.

Application/Uses:

  • Asphalt Modification
  • Assembly
  • Automotive
  • Bookbinding
  • Building and Construction
  • Caulks and Sealants
  • Contact Adhesives
  • Hot Melt Adhesives
  • Laminating
  • Nonwovens
  • Packaging
  • Pressure sensitive adhesives
  • Rubber and Plastic Modification
  • Solventborne Adhesives
  • Tapes and Labels
  • Wax Modification
  • Wire and Cable
Key Attributes:
  • Broad compatibility with numerous elastomers, polymers, and other tackifying resins
  • Consistent quality
  • Excellent heat stability
  • Light color
  • Low odor

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/cc
Brookfield Viscosity 350 cP
@Temperature 190 °C
Molecular Weight 550 g/molMn
 1100 g/molMw. Mw/Mn ratio = 2
 2250 g/molMz
 
Thermal PropertiesOriginal ValueComments
Ring & Ball Softening Point 115 °CASTM E 28
 
Optical PropertiesOriginal ValueComments
Yellow Index 9.0 %2 cm cell; ASTM E 313
 18 %5 cm cell; ASTM E 313
Gardner Color Number <= 1.0ASTM D6166
 2.0Molten
 
Descriptive Properties
Cloud Point<-50°COMSCP
 61°CDACP
 80°CMMAP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5301 / 222495

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.