MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lanxess Bayscript® Magenta BB liq Dye Mixture
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: General properties:
  • Highly purified, low salt grade azo reactive dye
  • Excellent filterability (0.45 µm)
  • Very good ozone fastness
  • Very reliable shade on different kinds of papers
  • Economical dye without compromising on performance
Applications:
  • Water-based inks
  • High quality thermal and piezo ink-jet printing
  • Photographic printing
  • Excellent match for red shade magenta photo inks

      Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH 4.0 - 8.0
Viscosity <= 10 cP
Surface Tension >= 50 dynes/cm
 
Chemical PropertiesOriginal ValueComments
Ionic Impurities - Cl (Chloride) <= 500 ppmIon content
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Component Elements PropertiesOriginal ValueComments
Calcium, Ca <= 0.0050 %Ion content
Iron, Fe <= 0.0010 %<10 ppm
Magnesium, Mg <= 0.0010 %<10 ppm
 
Descriptive Properties
AppearanceRed liquid
Content<50 ppmSulfate, Ion content
 13 percentdye content
Specifications<0.01% residueFilterability (0.45 µm filter)
 ±5%Color strength tolerance
 3Lightfastness

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY8451 / 208844

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.