MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ConocoPhillips Hydroclear® 460 Rolling Oil
Categories: Fluid; Lubricant

Material Notes: Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary additive chemistry and is recommended for use in a variety of rolling applications for nonferrous materials, such as aluminum, copper, brass and other copper alloys. Hydroclear Rolling Oil is nonstaining, does not contain zinc and provides very good wear protection for use in hydraulic systems. Hydroclear Rolling Oil also can be used as an exceptional bearing lubricant and as a roll-coating oil in most mill applications. Hydroclear Rolling Oil provides exceptional oxidation resistance, foam control, rust and corrosion protection and rapid low-temperature demulsibility. Hydroclear Rolling Oil exceeds the performance requirements of Vickers I-286-S and U.S. Steel 127 and 136. Hydroclear Rolling Oil in ISO viscosity grades 150, 320 and 460 exceeds the Morgan Construction Company lubricant specifications for use in No-Twist Rod Mills.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012, and branding was further reorganized in 2016. The Hydroclear® trade name is no longer in use but products may be available under different names.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.893 g/cc0.0323 lb/in³
Viscosity Measurement 100100Viscosity Index
Saybolt Viscosity at 100°F 2195 SUS2195 SUS
Saybolt Viscosity at 210°F 142 SUS142 SUS
Kinematic Viscosity at 40°C (104°F) 411 cSt411 cSt
Kinematic Viscosity at 100°C (212°F) 29 cSt29 cSt
Oxidative Stability 2000 hour2000 hourASTM D 943
ASTM Color 5.55.5
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 160 kg353 lb (mass)
Four Ball Wear 0.420 mm0.0165 in
 
Thermal PropertiesMetricEnglishComments
Pour Point -15.0 °C5.00 °F
Rotating Bomb Oxidation Test (RBOT) 600 min600 minASTM D 2272
Flash Point 288 °C550 °F
 
Descriptive Properties
ASTM Rust A&BPassASTM D665
Copper Corrosion1A
Emulsion Characteristics (40-40-0)15 minutes
Foam Control (Sequence I,II,III)0-0-0
FZGPass 12 Load StagesASTM D5182

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON125 / 75162

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.