MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Phillips 66 Triton® Low Temp NLGI Grade 1
Categories: Fluid; Lubricant; Lithium Gellant; Polyalphaolefin (PAO)

Material Notes: Triton Low Temp is a premium quality, synthetic, extreme pressure (EP) lithium grease developed to provide outstanding protection for lightly loaded industrial equipment, chassis parts and sliding mechanisms operating at moderate to very low temperatures. Triton Low Temp is manufactured with a low-viscosity synthetic polyalphaolefin (PAO) base oil and lithium 12-hydroxystearate soap thickener. It is fortified with extreme-pressure and antiwear additives plus rust and oxidation inhibitors to provide excellent wear protection, corrosion resistance and long service life. It has outstanding pumpability at low temperatures. It has been used successfully with conventional grease guns to lubricate ski lifts and similar equipment operating at temperatures as low as -48°C (-55°F).

Applications:

  • Plain and rolling-element bearings on pulleys and conveyors operating in arctic climates
  • Ski lift equipment
  • Sliding mechanisms on automobile seats and industrial equipment
  • Chassis parts on mobile equipment operating in arctic climates
Triton Low Temp is approved by General Motors Corporation under Part No. 9985377 for lubrication of the moving mechanisms for automobile seats and manual transmission shifters during vehicle assembly

Features/Benefits:

  • Outstanding pumpability at moderate to very low temperatures
  • Excellent protection in subzero weather
  • Excellent wear protection
  • Protects against rust and corrosion

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.863 g/cc0.0312 lb/in³
Viscosity Measurement 125125Index
Saybolt Viscosity at 100°F 135 SUS135 SUS
Saybolt Viscosity at 210°F 43 SUS43 SUS
Kinematic Viscosity at 40°C (104°F) 26.2 cSt26.2 cSt
Kinematic Viscosity at 100°C (212°F) 5.1 cSt5.1 cSt
Oxidative Stability 100 hour
@Pressure 0.0276 MPa
100 hour
@Pressure 4.00 psi
Pressure Drop; ASTM D942
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 250 kg551 lb (mass)ASTM D2596
Four Ball Wear <= 0.500 mm<= 0.0197 inScar Diameter; ASTM D2266
Penetration P(60), 1/10 mm 310 - 340310 - 340ASTM D217
Timken Test 4540 g10.0 lbOK Load; ASTM D2509
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -48.0 °C-54.4 °F
Dropping Point 200 °C392 °F
 
Descriptive Properties
ColorLight Amber
ThickenerLithium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON5148 / 198401

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.