MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Zircar Refractory Composites RS-99W Refractory Sheet
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Type RS-99W boards can be moistened with water and molded into any desired shape. After low temperature bake-out of 300°C (570°F) boards are unaffected by moisture.

Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.10 g/cc0.0759 lb/in³
Loss On Ignition 4.0 - 5.0 %4.0 - 5.0 %
Porosity 48 %48 %
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.0180 GPa2.61 ksiparallel to thickness
Compressive Yield Strength 25.6 MPa3710 psiat 10% deflection, parallel to thickness
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.047 J/g-°C0.2502 BTU/lb-°F
Melting Point >= 1800 °C>= 3270 °F
Maximum Service Temperature, Air 1650 °C3000 °F
Shrinkage  0.30 - 1.0 %
@Temperature 1200 °C,
Time 3600 sec
0.30 - 1.0 %
@Temperature 2190 °F,
Time 1.00 hour
 3.0 - 5.0 %
@Temperature 1200 °C,
Time 3600 sec
3.0 - 5.0 %
@Temperature 2190 °F,
Time 1.00 hour
 8.0 - 10 %
@Temperature 1600 °C,
Time 3600 sec
8.0 - 10 %
@Temperature 2910 °F,
Time 1.00 hour
 
Component Elements PropertiesMetricEnglishComments
Al2O3 >= 99 %>= 99 %
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zircar Refractory Composites RS-201 Refractory Sheet
Zircar Refractory Composites ASPA-1 Alumina-Silica Fiber Paper
Thermal Transfer Composites PRIMEX Cast™ MCX-1405™ Aluminum Silicon Carbide Composite, Reinforced
Crystex Composites Mykroy/Mycalex MM 1301 Molding Grade Glass-bonded Mica Composite
Zircar Refractory Composites RSLE-57 Refractory Sheet

CZRCI20 / 2883

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.