MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
NOVA Chemicals SCLAIR® FP026-F LMDPE Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Linear Medium Density Polyethylene (LMDPE), Film

Material Notes:

Octene Copolymer

Features:

  • Good stiffness
  • Easy processability
  • Moderate toughness and strength
  • Excellent seal properties

Additives:

  • Processing antioxidant
  • Polymer process aid
  • Antiblock (3500 ppm)

Applications:

  • Heavy duty shipping sacks requiring moderate toughness and high stiffness
  • Industrial packaging
  • Industrial liners
  • Construction film
  • Automatic packaging film

Film properties are typical of blown film extruded on a 2.5" extruder with 4" die and 35-mil die gap at a blow up ratio of 2.5:1, but are dependent upon operating conditions.

United States: SCLAIR FP026-F resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 3.2a, and may thus be used in the United States as an article or component of an article intended for use in contact with food, without temperature or food-type restrictions, subject to technical suitability.

NOVA Chemicals polyethylene resins are biologically and chemically inert.

Information provided by NOVA Chemicals®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.926 g/ccASTM D 792
Thickness 25.0 microns1 mil
 76.2 microns3 mil
Melt Index of Compound 0.80 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 11.0 MPa1 mil; ASTM D 882
 12.0 MPa3 mil; ASTM D 882
Film Tensile Strength at Yield, TD 12.0 MPa1 mil; ASTM D 882
 12.0 MPa3 mil; ASTM D 882
Film Elongation at Break, MD 490 %1 mil; ASTM D 882
 630 %3 mil; ASTM D 882
Film Elongation at Break, TD 680 %3 mil; ASTM D 882
 710 %1 mil; ASTM D 882
Elmendorf Tear Strength MD 295 g1 mil; ASTM D 1992
 1080 g3 mil; ASTM D 1992
Elmendorf Tear Strength TD 752 g1 mil; ASTM D 1922
 1467 g3 mil; ASTM D 1922
Dart Drop Test 156 g1 mil, F50; ASTM D 1709/A
 453 g3 mil, F50; ASTM D 1709/A
Film Tensile Strength at Break, MD 41.2 MPa3 mil; ASTM D 882
 42.5 MPa1 mil; ASTM D 882
Film Tensile Strength at Break, TD 33.1 MPa1 mil; ASTM D 882
 35.2 MPa3 mil; ASTM D 882
1% Secant Modulus, MD 230 MPa3 mil; ASTM D 882
 234 MPa1 mil; ASTM D 882
1% Secant Modulus, TD 251 MPa1 mil; ASTM D 882
 260 MPa3 mil; ASTM D 882
 
Optical PropertiesOriginal ValueComments
Haze 14 %
@Thickness 0.0254 mm
ASTM D 1003
 17 %
@Thickness 0.0762 mm
ASTM D 1003
Gloss 50 %@ 45°, 1 mil; ASTM D 2457
 61 %@ 45°, 3 mil; ASTM D 2457
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Low Friction Puncture (J/mm)20NOVA Chemicals Test Method, 3 mil
 25NOVA Chemicals Test Method, 1 mil

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOVB089 / 194697

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.