MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Phillips 66 Refrigerant Compressor Oil ISO Grade 100
Categories: Fluid; Lubricant

Material Notes: Refrigerant Compressor Oil is a highly refined naphthenic mineral oil developed primarily for use in reciprocating and rotary screw compressors in refrigeration systems using ammonia, carbon dioxide or non-HFC refrigerants. It also may be used as a general-purpose, light-duty lubricant for industrial machinery operating in cold environments. Refrigerant Compressor Oil is manufactured from carefully selected wax-free base stocks to have a low pour point and a low floc point for use in refrigeration system compressors. It has excellent low-temperature properties, good oxidation stability and low carbon-forming tendency to minimize deposit formation, provides good lubricity for protection against wear, and has excellent miscibility with non-HFC refrigerants. It also has good solvency and light color for use as a process oil or as a blending component in other lubricants. Refrigerant Compressor Oil meets the performance requirements of leading OEMs for use in refrigeration system compressors where the manufacturer specifies a naphthenic mineral oil.

Applications:

  • Compressors in refrigeration systems using ammonia, carbon dioxide or CFC or HCFC refrigerants, such as R-11, R-12, R-22 and R-502(1)
  • Plain and rolling-element bearings operating at low temperatures and under light loads
  • Drive chains
  • Process oil
Features/Benefits:
  • Excellent low-temperature properties
  • Wax-free
  • Good oxidation stability
  • Low carbon-forming tendency
  • Excellent miscibility with non-HFC refrigerants
  • Good lubricity
  • Good solvency
  • Light color

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.921 g/cc0.921 g/cc
Density 0.919 g/cc0.0332 lb/in³
Viscosity Measurement 2323Index
Saybolt Viscosity at 100°F 527 SUS527 SUS
Saybolt Viscosity at 210°F 54.6 SUS54.6 SUS
Kinematic Viscosity at 40°C (104°F) 98.9 cSt98.9 cSt
Kinematic Viscosity at 100°C (212°F) 8.4 cSt8.4 cSt
ASTM Color 3.03.0ASTM D1500
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.0500.050[mg KOH/g]; ASTM D974
 
Thermal PropertiesMetricEnglishComments
Pour Point -29.0 °C-20.2 °F
Flash Point 194 °C381 °FCOC
 
Descriptive Properties
Aniline Point82°CASTM D611
Carbon Residue0.08%ASTM D524
Floc Point-31°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ConocoPhillips Hydroclear® 320 Multipurpose R&O Oil, AGMA Lubricant No. 6
ConocoPhillips Conoco® El Mar® Geo Low Ash Oil, SAE Viscosity Grade 15W-40
ConocoPhillips Conoco® El Mar® Ashless Supreme Oil, SAE Viscosity Grade 15W-40
ChevronTexaco ISO 680 Ultra Gear Lubricant
ChevronTexaco ISO 680 AIO

WCON5038 / 198291

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.