MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
NUDEC® SANuv Acrylonitrile - Styrene Sheet
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Transparent

Material Notes: These plastic sheets are defined by many properties with special mention should be made of their good chemical resistance and mechanical strength. NUDEC® SANuv sheets incorporate UV additives that protect them from UV radiation, which allows them to maintain their optical properties in outside application for many years. These sheets possess excellent rigidity, even in small thicknesses. Because of their ease of handling, they are ideal for industrial parts, glazing, packaging and containers. Sheet properties: Excellent transparency and high brightness. Elevated rigidity and hardness. Good mechanical performance. Low water absorption. Good optical properties, long-term durable. Easy handling.

Information provided by NUDEC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 83
Ball Indentation Hardness 165 MPaISO 2039
Tensile Strength at Break 67.0 MPaISO 527
Elongation at Break >= 2.5 %ISO 527
Modulus of Elasticity 3.70 GPaISO 527
Flexural Strength 97.0 MPaISO 178
Charpy Impact Unnotched 17.0 kJ/m²ISO 179
Charpy Impact, Notched 1.29 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
CTE, linear >= 70.0 µm/m-°CISO 75-2
Maximum Service Temperature, Air 85.0 °C
Deflection Temperature at 0.46 MPa (66 psi) 101 °CHDT B; ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °CHDT A; ISO 75-2
Vicat Softening Point 105 °C
@Load 5.10 kg
ISO 306
 108 °C
@Load 1.02 kg
ISO 306
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.561ASTM D-542
Transmission, Visible 86 %ASTM D-1003
 
Descriptive Properties
Chemical ResistanceAcetic Acidregular
 Acetoneunsatisfactory
 Ammoniasatisfactory
 Detergentssatisfactory
 Ethanolregular
 Gasolinesatisfactory
 Glycerinsatisfactory
 Methanolregular
 Mineral oilsatisfactory
 Tolueneunsatisfactory
 Turpentineunsatisfactory
 vegetable oilsatisfactory
 Watersatisfactory
FlammabilityFrance, NFP 92-507, M4
 Germany, DIN 4102-1, B2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Peripor® 300 Expandable Polystyrene
PolyMirae Moplen EP3307 High Impact Polypropylene Copolymer
Overview of materials for Expanded Polystyrene (EPS)
NUDEC® PET Polyester Sheet
Overview of materials for Polypropylene, Molded

PNUDEC995 / 192061

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.