MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECAFORM® AH FG blue POM-C
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes:
  • food grade blue
  • low moisture absorption
  • easily machinable to tight tolerance
  • good mechanical properties
  • good wear properties
  • porosity free
Target Industries:
  • food processing
  • food technology
  • food engineering
  • packaging and paper machinery
  • conveyor technology
  • engineering for beverage filling systems
  • pharmaceutical industry

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³
Moisture Absorption 0.800 %0.800 %saturation; ASTM D570
 0.220 %
@Time 86400 sec
0.220 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8686ASTM D 785
Tensile Strength at Break 66.9 MPa9700 psiASTM D 638
Tensile Strength, Yield 60.7 MPa8800 psiASTM D 638
Elongation at Break 25 %25 %ASTM D 638
Elongation at Yield 9.0 %9.0 %ASTM D 638
Modulus of Elasticity 1.72 GPa250 ksiASTM D 638
Flexural Strength 82.7 MPa12000 psiASTM D 790
Flexural Modulus 2.76 GPa400 ksiASTM D 790
Compressive Yield Strength 79.3 MPa
@Strain 10 %
11500 psi
@Strain 10 %
ASTM D 695
Compressive Strength 8.27 MPa
@Strain 1 %
1200 psi
@Strain 1 %
ASTM D 695
Izod Impact, Unnotched 0.587 J/cm1.10 ft-lb/inASTM D 256
Coefficient of Friction, Dynamic 0.21
@Pressure 0.276 MPa
0.21
@Pressure 40.0 psi
50 fpm; ASTM D 3702
K (wear) Factor 131 x 10-8 mm³/N-M65.0 x 10-10 in³-min/ft-lb-hrAgainst Steel, 40 psi, 50 fpm; ASTM D 3702
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D 257
Dielectric Constant 3.7
@Frequency 60 Hz
3.7
@Frequency 60 Hz
50% RH; ASTM D 150
Dielectric Strength 19.7 kV/mm500 kV/inASTM D 149
Dissipation Factor  0.0010
@Frequency 60 Hz
0.0010
@Frequency 60 Hz
ASTM D 150
 0.0010
@Frequency 60 Hz
0.0010
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 84.6 µm/m-°C47.0 µin/in-°FASTM D 696
Melting Point 165 °C329 °F
Maximum Service Temperature, Air 90.6 °C195 °FLong Term
 141 °C285 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 158 °C316 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FASTM D 648
 
Descriptive Properties
Colorblue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8154 / 319082

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.