MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ChenGuang CGM 031-1 PTFE Powder for molding
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Description: PTFE powder for general moulding with medium particle size.

Physical and chemical properties:

  • Excellent chemical inertness.
  • Outstanding resistance to chemical corrosion, such as strong acid, alkali, strong oxidant, etc.
  • Exceptional resistance to high & low temperature, and to abrasion.
  • Can be used at temperature range from –200 ~ 250 °C for long period.
  • Superior electric insulation, which is not affected by temperature and frequency.
  • Non-adhesive to all other materials.
  • Non-absorption of moisture
  • Flame retardation.
Molecular formula: (CF2—CF2)n

Information provided by ChenGuang Research Institute of Chemical Industry

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.13 - 2.19 g/cc2.13 - 2.19 g/cc
Bulk Density 0.320 - 0.520 g/cc0.0116 - 0.0188 lb/in³
Particle Size 70 - 90 µm70 - 90 µm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 25.5 MPa>= 3700 psi
Elongation at Break >= 250 %>= 250 %
 
Thermal PropertiesMetricEnglishComments
Shrinkage <= 4.5 %<= 4.5 %
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.040 %<= 0.040 %
 
Descriptive Properties
ColorWhite powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHENGU016 / 255615

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.