MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik VESTAKEEP® 2000 FC30 PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: VESTAKEEP 2000 FC30 is a medium-viscosity, carbon fiber-reinforced, graphite and PTFE filled polyether ether ketone for injection molding. Parts made of this resin can be used for bearing bushing or gearbox parts, due to the self-lubricating effect. The semi-crystalline polymer features superior mechanical, thermal, and chemical resistance. Parts made from VESTAKEEP 2000 FC30 are self-extinguishing. VESTAKEEP 2000 FC30 can be processed by common injection-molding machines for thermoplastics. Manufacturer recommends a melt temperature between 370°C and 380°C during the injection molding process. If temperatures exceed 380°C, toxic gases can be released. Adequate ventilation and protective equipment must be provided.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.45 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0010 cm/cmdetermined on 2 mm sheets with film gate at rim mold temperature 180°C; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0040 cm/cmdetermined on 2 mm sheets with film gate at rim mold temperature 180°C; ISO 294-4
Melt Flow 15 g/10 min
@Load 5.00 kg,
Temperature 380 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 145 MPaISO 527-1
Elongation at Break 2.0 %ISO 527-1
Tensile Modulus 11500 MPaISO 527-1
Charpy Impact Unnotched 40.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 40.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 5.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 6.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+7 ohm-cmIEC 60093
Surface Resistance 1e+05IEC 60093
Dielectric Constant 4.9
@Frequency 1e+6 Hz
IEC 60250
 6.1
@Frequency 50 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359
Melting Point 340 °CISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 337 °CISO 75-1
Deflection Temperature at 1.8 MPa (264 psi) 320 °CISO 75-1
Vicat Softening Point 335 °C
@Load 5.10 kg
Method B; ISO 306
 340 °C
@Load 1.02 kg
Method A; ISO 306
Flammability, UL94 V-0
@Thickness 1.60 mm
IEC60695
Glow Wire Ignition Temperature 900 °C
@Thickness 2.00 mm
IEC 60695-2
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
IEC 60695-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 370 - 380 °C
Mold Temperature 160 - 200 °C
 180 °CPreferred

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik VESTAKEEP® 2000 CF30 PEEK
Evonik VESTAKEEP® 4000FC30 PEEK
LATI Larpeek 50 K/30 PEEK, 30% Carbon Fiber Reinforced
Akro-Plastic Akrotek® PEEK CF 30 black (5049) PEEK, Dry, 30% Carbon Filled
Ensinger Tecapeek® XP-98 Compression Molded PEEK Compound, 30% Carbon Fiber

PEVONIL206 / 196410

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.