MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

CHT CHT-BeauSil™ WAX 070 Silicone wax
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: Silicone waxes are more than an emollient in Personal Care. Silicone waxes are alkyl modified polydimethyl siloxanes that act different than classic silicone fluids in formulations. Outstanding performance is created by the alkyl modification which result in unique physical and chemical properties.

Key Features

  • Enhances spreading and solubilizing of natural lipids
  • Reduces tackiness
  • Provides controlled miniaturization
  • Dispersing and Solubilizing properties
Key Applications
  • Hair Care
  • Skin Care
  • Color Cosmetic
  • Sun Care
Application: CHT-BeauSil™ WAX 070 is a ideal ingredients for many types of skin care products, sun screens and colour cosmetics. A clear benefit beside the non-tacky and pleasant skin feeling is the high compatibility with organic ingredients and natural lipids. Additionally the CHT-BeauSil™ WAX 070 is a perfect wetting agent for pigments to create stable formulations. CHT-BeauSil™ WAX 070 can be used in leave-in products for hair care to improve softness and combing.

Addition Rates:
Dosage – 1: 0.5 – 5.0% as emollient
Dosage – 2: 0 – 10.0% as wetting agent for pigments
Dosage – 3: 1.0 – 5.0% as additive in sun screen

INCI Name: Cetyl dimethicone

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 0.00 %0.00 %
Brookfield Viscosity 40 - 120 cP40 - 120 cP
Storage Temperature 4.00 - 40.0 °C39.2 - 104 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceColorless to pale yellowish liquid
IonicityNon-ionic
MIT FreeYes
Ultralow cyclic contentYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL368 / 314851

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.