MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont™ Tedlar® TUT10BG3 UV Screening Transparent Polyvinyl Fluoride Film
Categories: Polymer; Film; Thermoplastic; Fluoropolymer

Material Notes: Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety of chemicals, solvents, and staining agents.

Key Words: PVF
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.37 g/cc1.37 g/ccASTM D1505
Moisture Absorption at Equilibrium <= 0.50 %<= 0.50 %ASTM D570
Moisture Vapor Transmission 0.760 cc-mm/m²-24hr-atm1.93 cc-mil/100 in²-24hr-atmASTM E96
Thickness 25.4 microns1.00 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD >= 95 %>= 95 %ASTM D882
Secant Modulus, MD 2.14 GPa310 ksiASTM D822
Impact 90.390.3kJ/m; Spencer; ASTM D3420
Coefficient of Friction 0.210.21Film:Metal; ASTM D1894
Tear Strength 144 kN/m822 pliGraves (initial), MD; ASTM D1004
 168 kN/m959 pliGraves (initial), TD; ASTM D1004
Elmendorf Tear Strength, MD 0.673 g/micron17.1 g/milASTM D1922
Elmendorf Tear Strength, TD 0.748 g/micron19.0 g/milASTM D1922
Film Tensile Strength at Break, MD >= 89.6 MPa>= 13000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
CTE, linear  78.0 µm/m-°C
@Temperature 50.0 - 70.0 °C
43.3 µin/in-°F
@Temperature 122 - 158 °F
MD; ASTM D696
 81.0 µm/m-°C
@Temperature 50.0 - 70.0 °C
45.0 µin/in-°F
@Temperature 122 - 158 °F
TD; ASTM D696
Specific Heat Capacity 1.76 J/g-°C0.421 BTU/lb-°FDuPont 990 test
Maximum Service Temperature, Air 107 °C225 °FContinuous
 175 °C347 °FShort Cycle
Minimum Service Temperature, Air -72.0 °C-97.6 °FContinuous
Shrinkage <= 6.0 %
@Temperature 170 °C
<= 6.0 %
@Temperature 338 °F
TD; ASTM D1204
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.46
@Temperature 30.0 °C
1.46
@Temperature 86.0 °F
nD; Abbe Refractometer; ASTM D-542
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Descriptive Properties
Aging in Air> 3000 hours to embrittlement300°F Oven

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont™ Tedlar® TTR10BG3 Transparent Polyvinyl Fluoride Film
DuPont™ Tedlar® SP TTR10SH9 Clear Polyvinyl Fluoride Film
DuPont™ Tedlar® SP TTR10AH9 Transparent Polyvinyl Fluoride Film
DuPont™ Tedlar® SP TTR5JAM9 Transparent Polyvinyl Fluoride Film
DuPont™ Tedlar® SP TUA10AH9 Polyvinyl Fluoride Film

PDU9307 / 138480

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.