MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

DuPont Mobility and Materials Rynite® FR530L BK507 Polyethylene Terephthalate (PET)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant

Material Notes:

Rynite FR530 BK507 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Key Words: PET-GF30FR(17)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.68 g/cc0.0607 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inISO 294-4 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 130 MPa18900 psiISO 527-1/-2
Elongation at Break 1.9 %1.9 %ISO 527-1/-2
Tensile Modulus 11.3 GPa1640 ksiISO 527-1/-2
Flexural Strength 200 MPa29000 psiISO 178
Flexural Modulus 10.5 GPa1520 ksiISO 178
Charpy Impact Unnotched 4.00 J/cm²19.0 ft-lb/in²ISO 179/1eU
 3.00 J/cm²
@Temperature -40.0 °C
14.3 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²4.28 ft-lb/in²ISO 179/1eA
 0.800 J/cm²
@Temperature -40.0 °C
3.81 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 225 V225 VIEC 60112
 250 - 400 V250 - 400 VUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 14.0 µm/m-°C7.78 µin/in-°FISO 11359-1/-2
 20.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
11.1 µin/in-°F
@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C50.0 µin/in-°FISO 11359-1/-2
 73.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
40.6 µin/in-°F
@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
Melting Point 252 °C486 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 243 °C469 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 220 °C428 °FISO 75-1/-2
UL RTI, Electrical 155 °C
@Thickness 0.400 mm
311 °F
@Thickness 0.0157 in
UL 746B
Flammability, UL94  V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
IEC 60695-11-10
 V-0
@Thickness 0.300 mm
V-0
@Thickness 0.0118 in
IEC 60695-11-10
 5VA
@Thickness 1.50 mm
5VA
@Thickness 0.0591 in
IEC 60695-11-20
 
Descriptive Properties
Part Marking Code>PET-GF30FR<ISO 11469
ProcessingInjection Molding
Regional AvailabilityEurope
 Near East/Africa
Resin IdentificationPET-GF30FR(17)
UL recognitionUL

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Rynite® FR530 BK507 PET-GF30FR(17)
DuPont Mobility and Materials Rynite® FR530L NC010 Polyethylene Terephthalate (PET)
Celanese Rynite® 408 NC010 PET
Celanese Rynite® 530HTE NC010 PET-GF30
Celanese Rynite® RE19051 BK507 Polyethylene Terephthalate (PET)

PZDSY5280 / 161107

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.