MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

CP-Polymer-Technik Wellamid® 6000 GV 15 HWCP 15% Glass Fiber Nylon 6, Heat Stabilized, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: Information provided by CP-Polymer-Technik GmbH & Co. KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ISO 1183
Moisture Absorption at Equilibrium 2.0 - 2.5 %2.0 - 2.5 %23°C/50%RH; DIN 53495
Linear Mold Shrinkage 0.0040 cm/cm
@Thickness 4.00 mm
0.0040 in/in
@Thickness 0.157 in
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
@Thickness 4.00 mm
0.0090 in/in
@Thickness 0.157 in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 125 MPa18100 psi5 mm/min; ISO 527
Elongation at Break 3.0 %3.0 %5 mm/min; ISO 527
Tensile Modulus 6.00 GPa870 ksiISO 527
Flexural Modulus 5.00 GPa725 ksiDIN 52457
Charpy Impact Unnotched 5.20 J/cm²
@Temperature 23.0 °C
24.7 ft-lb/in²
@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 93
Surface Resistance 1.00e+12 ohm1.00e+12 ohmISO 3915
Dielectric Constant 4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
IEC 250
Dielectric Strength 35.0 kV/mm889 kV/inIEC 243-1
Dielectric Loss Index 0.025
@Frequency 1e+6 Hz
0.025
@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 550 V550 VStufe; IEC 112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 35.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
19.4 µin/in-°F
@Temperature 73.4 - 176 °F
DIN 53752
Melting Point 215 °C419 °FKofler
Deflection Temperature at 0.46 MPa (66 psi) 215 °C419 °FISO 179
Deflection Temperature at 1.8 MPa (264 psi) 190 °C374 °FISO 179
Vicat Softening Point 200 °C392 °F50 N; ISO 306
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Stufe; IEC 707
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
Stufe; IEC 707
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 280 °C482 - 536 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
 
Descriptive Properties
Back PressureLow
Holding PressureHigh
Injection SpeedMedium to High
Screw SpeedHigh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWELL046 / 72503

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.