MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Solvay MIRATAINE® L-30 Surfactant  (discontinued **)
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Mirataine L-30 is a high foaming betaine surfactant that demonstrates excellent stability properties over broad pH range. Tipically used as a secondary surfactant in anionic based systems, MIRATAINE L-30 improves overall foam quality and also helps improve formulation mildness. Compliant with EU's detergent biodegradability regulation.

Identification: ALKYL DIMETHYL BETAINE

CAS: 66455 – 29 – 6

EINECS: 266 – 368 – 1

Compatibility: All surfactant classes

Use level: 1-10%

Available in: Asia Pacific, Europe, Latin America and North America

Applications: MIRATAINE L-30 is a high foaming betaine surfactant that demonstrates excellent stability properties over broad pH ranges. Typically used as a secondary surfactant in anionic based systems, MIRATAINE L-30 improves overall foam quality and also helps improve formulation mildness.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/cc
pH 6.0 - 8.05% Solution; RP-0420
 
Chemical PropertiesOriginal ValueComments
Ionic Impurities - Fe (Iron) <= 5.0 ppmRP-0277
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Component Elements PropertiesOriginal ValueComments
H2O, Water 60 - 64 %100-Solid; RP-0536
 
Descriptive Properties
AppearanceClear pale yellow liquid
Color<100APHA, RP-0134
CompositionActive29-31%, MMW=279, RP-1438
 Free Alkldimethylamine in Betaines<0.5%, RP-17512
 SMCA<100 ppm RP-0108
 Sodium Chloride6.5-7.5%, RP-0097

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WRHOD291 / 137522

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.