System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Lubrizol Estane® ZHF 90AT2 Thermoplastic Polyurethane
Categories:
Polymer
;
Thermoplastic
;
Polyurethane, TP
Material Notes:
Type: Estane® ZHF 90AT2 is a non-halogen, flame retardant, aromatic polyether-based thermoplastic polyurethane.
Application: Extrusion
Information provided by The 159 Corporation
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.24
g/cc
ISO 2781
Maximum Moisture Content
0.020
Mechanical Properties
Original Value
Comments
Hardness, Shore A
88
ISO 868
Tensile Strength
28.0
MPa
ISO 527-2/5A/200
Elongation at Break
520 %
ISO 527-2/5A/200
50% Modulus
8.00
MPa
@Strain 50 %
ISO 527-2/5A/200
100% Modulus
10.0
MPa
@Strain 100 %
ISO 527-2/5A/200
300% Modulus
14.0
MPa
@Strain 300 %
ISO 527-2/5A/200
Tear Strength
85.0
kN/m
Nicked; ISO 34-1B
Abrasion
90
[mm3]; ISO 4649-B
Thermal Properties
Original Value
Comments
Vicat Softening Point
85.0
°C
A50; ISO 306
Flammability, UL94
V-2
@Thickness 3.00 mm
Smoke Density
38
@Thickness 0.750 mm
Flaming DM; ASTM E662
112
@Thickness 0.750 mm
Non flaming DM; ASTM E662
Processing Properties
Original Value
Comments
Zone 1
200
°C
Zone 2
205
°C
Zone 3
210
°C
Zone 4
205
°C
Adapter Temperature
205
°C
5
Die Temperature
200
°C
Tip
205
°C
Drying Temperature
82.0
°C
@Time 7200 - 14400 sec
Dew Point
-40.0
°C
Component Elements Properties
Original Value
Comments
Loss on Ignition(%)
24 %
ASTM D-2863
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PLUBR5028 / 238898
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.