MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Westlake HIFOR SC74580 Clear LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: HIFOR Clear Polyethylene SC74580 polymer is a high strength and high clarity linear low density polyethylene designed for blown film extrusion that contains no slip and no antiblock. It does contain processing aid. Blown films produced with this resin exhibit good toughness, with exceptional gloss and clarity for a product of this density, yet film blocking is substantially lower than one might expect. Film stiffness is also higher than one might expect for this density. It works well in many shrink film applications. Gauge of test specimens 1.0 mil fabricated on a 6” die, 2.5” 24:1 L:D barrier screw, 2.4:1 BUR, 100-mil die gap, 15” frostline height, 450º F melt temperature, and 7.5 lb/hr/inch die output. Density results are on Base Resin. This product has some 21 CFR clearances. Application/Uses: Frozen food films- High clarity bread bags- Ice bags.

Samples tested at 23°C and 50% RH.

Information provided by Westlake Chemical Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.926 g/ccASTM D1505
Melt Index of Compound 0.60 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 600 %ASTM D882
Film Elongation at Break, TD 950 %ASTM D882
Dart Drop 100 g/milASTM D1709
Film Tensile Strength at Break, MD 8200 psiASTM D882
Film Tensile Strength at Break, TD 5500 psiASTM D882
1% Secant Modulus, MD 47000 psiASTM D882
1% Secant Modulus, TD 55000 psiASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 4.0 %ASTM D1003
Gloss 82 %@ 45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 400 - 420 °Fblown film
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Westlake HIFOR SC74558 Clear LLDPE

PWESF8836 / 222908

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.