MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik P84®NT1 05P DF Aromatic Polyimide
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes:
  • Excellent performance at high temperatures
  • High strength and excellent shape stability
  • Very good impact resistance
  • High heat deflection temperature
  • Very good creep resistance even at elevated temperatures
  • Machinable with standard tools
  • Low wear and friction behavior
  • Processing by Hot compression molding
Application examples: bushings, seals, bearings components, guides, gear wheels, and valve parts in the automotive and aerospace industries and in industrial equipment.
Industrial Sector: Automotive and Mobility, Aircraft and Aerospace, Industry and Engineering
Processing: Press and sintering, Machining
Delivery form: Pellets, Granules, Powder
Resistance to: Heat (thermal stability), Fire / burn, Wear / abrasion, Oil / fuels
Electrical: Insulating
Additives: Release agent, Unfilled
Applications: Displays, Electrical and Electronical, General purpose, Fittings
Processing: DF Direct forming
Special Characteristics: Amorphous, High heat resistant, Non-dripping, Self-extinguishing
Features: Creep resistance, Low coefficient of friction, Lightweight
Color: Natural color, Yellow
Additives: Release agent
Chemical Resistance: Acid resistance, Solvent resistance, Grease resistance, Oil resistance, Radiation resistance, Fuel resistance

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.400 g/cc0.0145 lb/in³EN ISO 60
Density 1.28 g/cc0.0462 lb/in³ISO 1183
Water Absorption  1.40 %
@Time 86400 sec
1.40 %
@Time 24.0 hour
ISO 62
 1.90 %
@Time 173000 sec
1.90 %
@Time 48.0 hour
ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 84.084.0ISO 7619-1
Tensile Strength at Break 74.0 MPa10700 psiISO 527
Tensile Strength 74.0 MPa10700 psiISO 527
Elongation at Break 3.70 %3.70 %ISO 527
Tensile Modulus 2.92 GPa424 ksiISO 527
Flexural Strength 110 MPa16000 psiISO 178
 110 MPa16000 psiat break; ISO 178
Flexural Modulus 2.88 GPa418 ksiISO 178
Flexural Strain at Break 4.30 %4.30 %ISO 178
Compressive Strength 392 MPa56900 psiISO 604
Compressive Modulus 3.08 GPa447 ksiISO 604
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmon bar, ?V; Sim. to IEC 62631-3-1
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmRSD; IEC 62631-3-2
Dielectric Constant 3.40
@Frequency 100 Hz
3.40
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 34.0 kV/mm
@Thickness 1.00 mm
864 kV/in
@Thickness 0.0394 in
AC, S20/S20, t; IEC 60243-1
Dissipation Factor 0.0000400
@Frequency 100 Hz
0.0000400
@Frequency 100 Hz
IEC 62631-2-1
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.980 J/g-°C0.234 BTU/lb-°FISO 22007-4
Thermal Conductivity 0.230 W/m-K1.60 BTU-in/hr-ft²-°FISO 22007-4
Deflection Temperature at 0.46 MPa (66 psi) 320 °C608 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 307 °C585 °FISO 75-1/-2
Glass Transition Temp, Tg 326 °C619 °FISO 11357-1/-2
Flammability, UL94 V-0
@Thickness 0.762 mm
V-0
@Thickness 0.0300 in
IEC 60695-11-10
 
Descriptive Properties
ColorNatural color, Yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7810 / 324942

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.