MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Nickel Aluminum Bronze, UNS C63200
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Good to excellent corrosion resistance. Good hot formability. Fabricated by hot forming and welding.

Applications: nuts, bolts, structural pump parts, shafting requiring corrosion resistance.

Available as rod, bar, and forgings.

Key Words: Copper, CDA 632
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.64 g/cc0.276 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 92 - 9792 - 97
Tensile Strength, Ultimate 640 - 725 MPa92800 - 105000 psiDepending on amount of cold work or heat treatment
Tensile Strength, Yield 330 - 380 MPa47900 - 55100 psiDepending on amount of cold work or heat treatment
Elongation at Break 18 %18 %in 50 mm, 18% reduction in area
Modulus of Elasticity 115 GPa16700 ksi
Compressive Strength 760 MPa110000 psi
Poissons Ratio 0.320.32
Machinability 30 %30 %Based on 100% machinability for UNS C360000
Forgeability 70 %70 %
Shear Modulus 44.0 GPa6380 ksi
Charpy Impact  13.0 - 16.0 J
@Temperature -29.0 - 20.0 °C
9.59 - 11.8 ft-lb
@Temperature -20.2 - 68.0 °F
Keyhole
 23.0 - 27.0 J
@Temperature -29.0 - 20.0 °C
17.0 - 19.9 ft-lb
@Temperature -20.2 - 68.0 °F
V-notch
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000246 ohm-cm
@Temperature 20.0 °C
0.0000246 ohm-cm
@Temperature 68.0 °F
Magnetic Permeability 1.041.04
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
9.00 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.439 J/g-°C0.105 BTU/lb-°F
Thermal Conductivity 36.0 W/m-K
@Temperature 20.0 °C
250 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1040 - 1060 °C1900 - 1940 °F
Solidus 1040 °C1900 °F
Liquidus 1060 °C1940 °F
Annealing Point 621 - 704 °C1150 - 1300 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 705 - 880 °C1300 - 1620 °F
Hot-Working Temperature 705 - 925 °C1300 - 1700 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 8.0 - 9.5 %8.0 - 9.5 %
Copper, Cu 75.9 - 84.5 %75.9 - 84.5 %
Iron, Fe 3.0 - 5.0 %3.0 - 5.0 %
Lead, Pb <= 0.020 %<= 0.020 %
Manganese, Mn <= 3.5 %<= 3.5 %
Nickel, Ni 4.0 - 5.5 %4.0 - 5.5 %
Other, total <= 0.50 %<= 0.50 %
Silicon, Si <= 0.10 %<= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nickel Aluminum Bronze, UNS C63000, Annealed Rod
Aluminum Bronze, UNS C95400, Copper Casting Alloy, As Cast
Alpha Nickel-Aluminum Bronze, UNS C95800, Copper Casting Alloy
Nickel Aluminum Bronze, UNS C63000, HR50 Temper
Copper, UNS C62400 (Aluminum Bronze 11%)

MC63200b1 / 11612

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.