MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess Aflux® 54 Processing Aid
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Function: Processing promoter for compounds based on synthetic rubber, especially CO, ECO and FKM

Use Aflux 54 decreases the viscosity of rubber compounds, resulting in an easier processing and a faster compounding. Aflux 54 noticeably reduces the sticking of the compounds to the mixing units. It improves the absorption of all kinds of fillers and the extrusion properties of the compounds. The vulcanizate properties are not impaired by Aflux 54. Aflux 54 promotes the demolding of press-cured articles and reduces mold fouling.

Application: Particularly suitable for AU, CO, ECO and FKM, technical molded and extruded articles. Reduces the viscosity of rubber mixes. Reduces sticking to mixer units, aids removal of vulcanizates from the mold.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³
 
Thermal PropertiesMetricEnglishComments
Melting Point 58.0 - 65.0 °C136 - 149 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 36.0 Month36.0 Month
 
Descriptive Properties
Appearanceoff-white micro pearls

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8246 / 208639

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.