Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. It has improved stiffness through the addition of 20 % filler. Improved stiffness and high fluidity realizes a thin wall of OA machines etc. Applications: Thin wall components of mechanical, electric and electronic equipment that need least warpage and dimensional accuracy etc.Information provided by Teijin Chemicals Ltd. |