MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LyondellBasell Hifax™ CA45 Thermoplastic Olefin Resin  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes:
Key Features: medium melt flow, medium modulus thermoplastic elastomeric olefin resin, excellent balance of properties, excellent processability, good colorability, excellent surface appearance

Applications: molded-in color automotive bumper fascias and step pads, air deflectors, appliques

Description: Hifax CA45 medum melt flow, reactor grade thermoplastic elastomeric olefin resin has a very good balance of properties and excellent moldability. It was designed primarily for molded-in color automotive exterior components and is based on material from Montell's Spheripol process.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc0.0322 lb/in³ISO 1183
Linear Mold Shrinkage 0.013 cm/cm0.013 in/inTool, Montell
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
9.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ISO 868
Tensile Strength, Ultimate 8.00 MPa1160 psiISO R527-1
Tensile Strength, Yield 17.0 MPa2470 psiISO R527-1
Elongation at Break 500 %500 %ISO R527-1
Elongation at Yield 16 %16 %ISO R527-1
Flexural Modulus 0.820 GPa119 ksiISO 178
Izod Impact, Notched 0.700 J/cm
@Temperature -40.0 °C
1.31 ft-lb/in
@Temperature -40.0 °F
ISO 180
Impact Test 25.0 J
@Temperature -30.0 °C
18.4 ft-lb
@Temperature -22.0 °F
MAII, E at Max Load, Ductile; ISO 6603-2
 
Thermal PropertiesMetricEnglishComments
CTE, linear 100 µm/m-°C
@Temperature -30.0 - 30.0 °C
55.6 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 63.0 °C145 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 43.0 °C109 °FISO 75

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hifax™ CA10GC Thermoplastic Polyolefin Elastomer
LyondellBasell Dexflex 980 BLK Thermoplastic Polyolefin
LyondellBasell Dexflex 810 BLK Thermoplastic Polyolefin
LyondellBasell Hifax™ CA187 Thermoplastic Olefin Resin
LyondellBasell Hifax™ CA244 Thermoplastic Polyolefin Elastomer

PMO447 / 53638

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.