MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Ho Hsiang Ching H-950N SEBS
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: The material is translucent and light gravity, its good coloring and elastic properties which give the product a cushioned feel and the broad range of hardness can reach SHORE 30A~ SHORE 60D. For example, the pliers handles, need to have a highly resilient force in using, it means that the user doesn’t need to put much strength by hand. A full elasticity handle made of great specific materials, it not only makes the tool easier to use, but also gives it a more ergonomic design.

Color: Translucent

The optimum combination of materials: PP, PE, EVA

Processing: Injection, Extrusion

Storage conditions: At room temperature, avoid direct sunlight, keep away from fire and avoid humid environment.

Applications: Pliers

Information provided by Ho Hsiang Ching Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.880 g/cc0.880 g/ccASTM D792
Melt Flow 20 - 30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
20 - 30 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9595ASTM D2240
Tensile Strength 7.85 MPa1140 psiASTM 412C
Elongation at Break 500 %500 %ASTM 412C
Tear Strength 63.7 kN/m364 pliASTM 412C
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 70.0 °C158 °F
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 160 - 177 °C320 - 351 °F
Middle Barrel Temperature 166 - 182 °C331 - 360 °F
Front Barrel Temperature 177 - 191 °C351 - 376 °F
Nozzle Temperature 182 - 204 °C360 - 399 °F
Mold Temperature 16.0 - 66.0 °C60.8 - 151 °F
Injection Velocity 13.0 - 25.0 mm/sec0.512 - 0.984 in/sec
Injection Pressure 34.0 - 69.0 MPa4930 - 10000 psi
Hold Pressure 14.0 - 48.0 MPa2030 - 6960 psi
Back Pressure 0.340 - 0.690 MPa49.3 - 100 psi
Screw Speed 50 - 70 rpm50 - 70 rpm
 
Descriptive Properties
Cold resistance temperature-40°C
ColorTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHSIANG024 / 312500

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.