MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Syensqo (Solvay Specialty Polymers) AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK), 30% carbon fiber
Categories: Polymer; Thermoplastic; Polyketone; Polyaryletherketone (PAEK), Carbon Fiber Filled

Material Notes: 30% carbon fiber, low melt flow for extrusion and injection molding

AvaSpire® AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 grade offers the highest strength, stiffness, and fatigue resistance of any AV-621 based grade. Furthermore, this resin generally retains most of the desirable ultra-performance attributes of carbon fiber reinforced PEEK including chemical resistance, fatigue resistance, and long term thermal oxidative stability.

The excellent balance of properties of AV-621 CF30 makes this grade well suited for a broad range of applications across a number of industries, including healthcare, transportation, electronics, and chemical processing.

This resin can be easily melt processed by injection molding using standard equipment. The melt processing behavior of AV-621 CF30 is very similar to that of 30% CF reinforced PEEK. The lower melt flow of AV-621 CF30 is well suited for extrusion applications while offering a similar property profile to AV-651 CF30.

Markets/Uses: Healthcare / Medical Devices / Medical Pump Seals; Healthcare / Medical Devices / Medical Reusable; Healthcare / Medical Devices / Medical/Healthcare Applications; Healthcare / Medical Devices / Orthopedics; Healthcare / Medical Devices / Packaging, Rigid Medical; Healthcare / Medical Devices / Sizing Trials; Healthcare / Medical Devices / Surgical Instruments; Miscellaneous / Industrial / Compressor Components; Oil & Gas / Down Hole / Compressor Components

Applications: Medical/Healthcare Applications; Pump Parts; Seals

Features: Chemical Resistant; Fatigue Resistant; Flame Retardant; Good Dimensional Stability; High Heat Resistance; High Stiffness; High Strength

Injection notes: Back Pressure: Minimum

Information provided by Solvay Specialty Polymers.

Vendors: Drake extrudes shapes and machines and injection molds parts in Torlon® PAI, PEEK, PAEK, Ryton PPS and Ultem PEI. It also machines Vespel® PI. Innovations include cryogenic CryoDyn® CT-200 shapes as a PCTFE alternative; efficient Seamless Tube® and the largest extruded rod diameters to >254mm and plate thicknesses to > 100mm. Certified to ISO 9001:2015 and AS9100D. Visit www.DrakePlastics.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³ASTM D792
Water Absorption 0.10 %
@Time 86400 sec
0.10 %
@Time 24.0 hour
ASTM D570
Viscosity 790 cP
@Shear Rate 1000 1/s,
Temperature 400 °C
790 cP
@Shear Rate 1000 1/s,
Temperature 752 °F
Melt; ASTM D3835
Linear Mold Shrinkage, Flow <= 0.0020 cm/cm
@Thickness 3.18 mm
<= 0.0020 in/in
@Thickness 0.125 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0090 - 0.011 cm/cm
@Thickness 3.18 mm
0.0090 - 0.011 in/in
@Thickness 0.125 in
ASTM D955
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 400 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 752 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 101101ASTM D785
Tensile Strength 181 MPa26300 psi5.0 mm/min; ASTM D638
Tensile Strength, Yield 196 MPa28400 psiType 1A, 5 mm/min; ISO 527-2
Elongation at Break 2.2 %2.2 %5.0 mm/min; ASTM D638
 2.2 %2.2 %Type 1A, 5 mm/min; ISO 527-2
Tensile Modulus 17.2 GPa2490 ksi5.0 mm/min; ASTM D638
 23.3 GPa3380 ksi1 mm/min, Type 1A; ISO 527-2
Flexural Strength 276 MPa40000 psiASTM D790
 296 MPa42900 psiISO 178
Flexural Modulus 15.1 GPa2190 ksiASTM D790
 21.3 GPa3090 ksiISO 178
Compressive Strength 152 MPa22000 psiASTM D695
Shear Strength 91.0 MPa13200 psiASTM D732
Izod Impact, Notched 0.690 J/cm1.29 ft-lb/inASTM D256
Izod Impact, Unnotched 6.40 J/cm12.0 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 9.60 kJ/m²4.57 ft-lb/in²ISO 180
Izod Impact, Unnotched (ISO) 39.0 kJ/m²18.6 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 5.00 µm/m-°C
@Temperature -50.0 - 50.0 °C
2.78 µin/in-°F
@Temperature -58.0 - 122 °F
ASTM E831
Specific Heat Capacity  1.35 J/g-°C
@Temperature 50.0 °C
0.323 BTU/lb-°F
@Temperature 122 °F
ASTM C351
 1.81 J/g-°C
@Temperature 200 °C
0.433 BTU/lb-°F
@Temperature 392 °F
ASTM C351
Thermal Conductivity 0.350 W/m-K2.43 BTU-in/hr-ft²-°FASTM C177
Melting Point 340 °C644 °FPeak; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
@Thickness 3.20 mm
410 °F
@Thickness 0.126 in
Annealed; ASTM D648
Glass Transition Temp, Tg 160 °C320 °FDSC
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 366 °C691 °F
Middle Barrel Temperature 371 °C700 °F
Front Barrel Temperature 377 °C711 °F
Nozzle Temperature 382 °C720 °F
Melt Temperature 366 - 388 °C691 - 730 °FInjection
Mold Temperature 149 - 177 °C300 - 351 °F
Drying Temperature 149 °C
@Time 14400 sec
300 °F
@Time 4.00 hour
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormsPellets
Injection RateFast
ProcessingInjection Molding; Machining; Profile Extrusion
Screw Compression Ratio2.0:1.0 to 3.0:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4147 / 279947

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.