MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Hexcel® HexWeb® CR-PAA™ 3/8-5052-0.002 Phosphoric Acid Anodized Aluminum Honeycomb
Categories: Metal; Metal Foam, Mesh, or Honeycomb; Nonferrous Metal; Aluminum Alloy; 5000 Series Aluminum Alloy

Material Notes: Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the face sheets that carry bending loads and the honeycomb that carries the shear loads. The adhesive is the interface between the facing and the core in the same way that the oxide on the aluminum and the primer that has been applied to it is the interface between the honeycomb substrate material and the bonding adhesive. This interface is critical to the performance of honeycomb bonded assemblies.

HexWeb® CR-PAA™ is designed for aircraft structures that are exposed to demanding environmental conditions. HexWeb® CR-PAA™ outperforms standard MIL-C-7438 core in salt spray and HexWeb® crack propagation tests.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.00 lb/ft³Nominal
 
Mechanical PropertiesOriginal ValueComments
Compressive Yield Strength >= 0.190 ksiBare, min
 >= 0.200 ksiStabilized, min
 0.285 ksiBare, typical
 0.310 ksiStabilized, typical
Compressive Modulus 70.0 ksiStabilized, typical
Shear Modulus 21.2 ksiPlate Shear, W Direction, typical
 43.0 ksiPlate Shear, L Direction, typical
Shear Strength >= 0.0850 ksiPlate Shear, W Direction, min
 0.125 ksiPlate Shear, W Direction, typical
 >= 0.145 ksiPlate Shear, L Direction, min
 0.200 ksiPlate Shear, L Direction, typical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexForce™ GA120 Carbon Fabric
Toho Tenax Besfight® G30-500 12K HTA-7C EP03 Continuous Filament Carbon Fiber
Solvay Thornel® T-300 1K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Hexcel® HexWeb® HRH-10 - 3/8 - 1.5 Aramid Fiber/Phenolic Resin Honeycomb
DowAksa AKSACA™ A-49 D 12K Continuous Carbon Fiber

PHEXC289 / 98760

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.